Greene Tweed Arlon® 1000 Polyketone

 

Subcategory: Polyketone; Thermoplastic

Material Notes:
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprietary manufacturing and machining processes to ensure that Arlons properties consistently outperform the competition.

Greene, Tweed offers several different Arlon materials, and all provide high tensile strength and elongation properties, excellent shear strength and creep resistance, outstanding fatigue resistance, broad chemical and radiation resistance, and no susceptibility to hydrolysis (steam/hot water). Our engineers work one on one with customers to find the right solution for each specific application.

Available Properties
  • Specific Gravity
  • Deformation
  • Hardness, Rockwell M
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Tensile Strength @ Break
  • Tensile Strength @ Yield
  • Elongation at Break
  • Flexural Modulus
  • Flexural Strength
  • Compressive Strength
  • Shear Strength
  • Secant Modulus
  • Coefficient of Friction
  • K (wear) Factor
  • CTE, linear, 212°F (100°C)
  • CTE, linear, 482°F (250°C)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。