Greene Tweed Avalon® 56 PTFE

 

Subcategory: Fluoropolymer; Thermoplastic; PTFE

Material Notes:
PTFE is preferred for use in many pharmaceutical-sealing applications. Its chemical inertness and ultra-low level extractables provide pharmaceutical process and validation engineers with a safe material to use in almost any applications. PTFE is visco-elastic, providing a functional seal when other fluorinated plastics such as PFA or FEP cannot. However, because virgin PTFE will creep under load its ability to provide a reliable seal during temperature cycling is limited.

Ferrule gaskets made from Avalon® 56 provide a level of performance superior to other PTFE materials used in the pharmaceutical and hygienic fluid handling industries. Greene Tweed’s Avalon 56 uses the latest generation modified PTFE. Modified PTFE contains a small amount of a perfluoroether to improve creep resistance, compressive strength and permeation resistance. Modified PTFE is not only the material of choice for PTFE-faced diaphragm materials, but it is also FDA compliant.

While other gasket manufacturers fabricate gaskets by directly molding the finished part, Greene Tweed machines Avalon 56 sanitary gaskets and custom shapes from isostatic-molded billets to provide optimal physical properties and tighter tolerances, easing the installation process.

Avalon 56 virgin PTFE seals deliver improved sealing performance over standard PTFE

Avalon 56 is available in all sanitary gasket sizes, as well as custom shapes.

Information provided by Green Tweed

Available Properties
  • Specific Gravity
  • Deformation
  • Tensile Strength @ Yield
  • Elongation at Break
  • Shear Strength
  • Coefficient of Friction
  • Coefficient of Friction, Static
  • K (wear) Factor
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。