EMS-Grivory Grilamid® TR55 LZ Transparent Nylon 12, As Conditioned

 

Subcategory: Nylon; Thermoplastic; Nylon 12

Material Notes:
Grilamid TR 55 LZ is a specially modified grade of Grilamid TR 55 (amorphous nylon 12 based material) which provides exceptional toughness and resistance to chemicals, including alcohol and other cleaning agents. Because it is heat and light stabilized, Grilamid TR 55 LZ offers excellent resistance to stress cracking and retains its properties even after prolonged exposure to weathering and high temperatures.

Grilamid TR 55 LZ may be considered for a variety of consumer and industrial applications in which chemical resistance, transparency and toughness are desired. Grilamid TR 55 LZ offers low moisture absorption and dimensional stability with the highest impact strength of the Grilamid TR 55 grades.

Grilamid TR 55 LZ contains no plasticiser, resists cosmetic chemicals and perspiration, does not irritate the skin and can enhance design and performance of personal care products such as sport and safety spectacle frames.

Information provided by EMS-Grivory

Available Properties
  • Density
  • Water Absorption
  • Water Absorption at Saturation
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Hardness, Shore D
  • Tensile Strength at Break
  • Elongation at Break
  • Elongation at Yield
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor, Low Frequency
  • Comparative Tracking Index
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Glass Temperature
  • Refractive Index
  • Transmission, Visible
  • Processing Temperature
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Die Temperature
  • Melt Temperature
  • Mold Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。