EMS-Grivory Grivory® XS 1363 Partially Aromatic Nylon, As Conditioned

 

Subcategory: Nylon; Thermoplastic; Nylon, Aromatic; Polymer

Material Notes:
Grivory XS 1363 is a 50% glass fiber reinforced, partially aromatic nylon. Designed specifically for the aircraft industry. Grivory XS 1363 exhibits good injection moldability and less tool abrasion than other comparably filled nylons. Like most nylons, Grivory XS 1363 has good chemical resistance.

Using Grivory XS 1363 instead of aluminum or magnesium offers many advantages; lower weight, corrosion free and little or no finishing (cleaning, machining, deflashing, painting, etc). In addition, tool life span for Grivory is greater than that of a metal die cast tool. These advantages over die cast metals lead to lower production costs, typically between 20 and 50 percent.

Grivory XS 1363 is suitable for use in interior aircraft cabin applications. Its high strength and stiffness is virtually unaffected by moisture , this combined with a good surface finish makes it ideal for applications such as: armrests, spreaders, tray brackets, overhead bin brackets, etc.

Information provided by EMS-Grivory

Available Properties
  • Density
  • Water Absorption
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Hardness, Shore D
  • Tensile Strength at Break
  • Elongation at Break
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Melt Temperature
  • Mold Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。