PolyOne ECCOH™ 0521-48 Low Smoke Free Of Halogen (LSFOH)

 

Subcategory: Thermoplastic

Material Notes:

ECC0H non-halogenated flame-retardant polyolefin compounds are ideal for applications that require non-corrosive materials such as mass transit, tunnels, and airports. Originally designed to meet European requirements in the transportation industry, these compounds are used for both sheathing and primary insulation. Specially designed for thin wall extrusion wire and cable applications, ECC0H compounds are low smoke and highly flame-retardant, and will not emit corrosive gasses when burned.

Description/Features:

  • Non-Halogenated
  • Low Smoke
  • Flame Retardant

Applications:

  • Thin-wall extrusion applications (Tape, x-web)

Market:

  • Wire & Cable

Processing Method:

  • Extrusion

TENSILE AND ELONGATION VALUES ARE LARGELY DETERMINED BY PROCESSING PARAMETERS OF THE END USER. NOTE: Tensile property data is from extruded tape 3:1 drawdown ratio and .006 in. NOTE: Dielectric Constant is measured on .085" plaque).PolyOne First Choice

Disclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Information provided by PolyOne Corporation.

Available Properties
  • Specific Gravity
  • Melt Flow
  • Tensile Strength @ Yield
  • Elongation at Break
  • Dielectric Constant
  • Oxygen Index
  • Appearance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。