PolyOne Geon® XV3432 Vinyl Compound - Flexible (FPVC)

 

Subcategory: Vinyl; Thermoplastic

Material Notes:

Description/Features:

  • Transparent

Applications:

  • FDA (Food Contact)
  • Hose and Tubing

Processing Method:

  • Extrusion and Molding
PolyOne First Choice

Disclaimer: NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is “For foods of high water content only”. This statement is only an overview of the FDA listings for this product. It is the customer's responsibility to ensure that the compound is suitable for its intended application.

Information provided by PolyOne Corporation.

Available Properties
  • Specific Gravity
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Brittleness Temperature
  • Product Form
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。