PolyOne Nymax® 1200 A L Black 13A Nylon 6/6

 

Subcategory: Nylon; Thermoplastic; Nylon 66

Material Notes:

The Nymax® 1200 Blend Series of nylon 6/6 materials are "salt-and-pepper" pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials have been formulated to provide improved melt processing, part performance, or surface appearance depending upon grade selected and are offered as an economical alternative to fully compounded products.

Description/Features:

  • Nylon 6/6 Blend
  • Lubricated
  • Black

Applications:

  • Multi-Purpose

Market:

  • Automotive
  • Building and Construction
  • Industrial
  • Consumer Goods

Processing Method:

  • Injection Molding

Molded Test Bars: (Dry as molded:PolyOne First Choice

Information provided by PolyOne Corporation.

Available Properties
  • Specific Gravity
  • Water Absorption
  • Linear Mold Shrinkage
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • Melting Point
  • Deflection Temperature at 1.8 MPa (264 psi)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。