PolyOne Teslart™ PUD-1 Teslart ICP/Aqueous Polyurethane

 

Subcategory: Additive/Filler for Polymer

Material Notes:

Description/Features:

  • A dispersion of Teslart Inherently Conductive Polymer and an aqueous polyurethane binder.

Applications:

  • Designed as a starting point for formulation for formulators requiring a conductive coating
  • Anti-fouling Marine Coatings
  • Antistatic Fabrics, Coatings and Packaging
  • Batteries
  • Conductive Inks and Adhesives
  • EMI/RFI Shielding
  • Radar / Microwave Absorption and Sensors

Custom dispersions can be created to meet a desired surface resistivity value or other physical characteristics. Please contact your PolyOne representative for more details.

Disclaimer: Material should remain sealed in storage. Avoid freezing.
Teslart ICP's are made under license of NASA's U.S. Patent Nos. 5,968,417; 6,059,999; 6,299,800 and other patents pending.

Information provided by PolyOne Corporation.

Available Properties
  • Specific Gravity
  • Solids Content
  • pH
  • Brookfield Viscosity
  • Surface Resistivity per Square
  • Active Ingredient
  • Binder/Vehicle
  • Color
  • Product Form
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。