PolyOne® 2116 Black PEC Black Polyethylene

 

Subcategory: Polyethylene; Additive/Filler for Polymer; Thermoplastic

Material Notes:

This concentrate has been designed for in-plant blending with appropriate natural high density polyethylene pipe resins to produce pipe with PE 2406 or PE 3408 ratings. 2116 Black PEC is manufactured to produce pipe free of surface imperfections with minimum screen pack plugging during extrusion. The carrier resin and stabilization system has been selected to maximize the physical and environmental properties of the pipe. A furnace carbon black has been selected to maximize processibility, while providing good outdoor weathering capability.

Description/Features:

  • Exterior-Weatherable
  • Black

Applications:

  • Pipe-Pressure
  • Pipe Fittings
  • Pipe Coupling

Processing Method:

  • Extrusion and Molding

Note: In order to meet requirements of the Plastics Pipe Institute (PPI), the pressure performance of pipe extruded from these blends must be verified. In-plant blending conditions and quality control procedures are important to achieve quality product, which will continue to meet these conditions. 2116 Black PEC is designed to be used at a 6.5% letdown rate in PPI TR-4 listed blends.

Information provided by PolyOne Corporation.

Available Properties
  • Carbon Black Loading
  • Melt Flow
  • Carrier
  • Product Form
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。