Degussa Plexiglas® zk6BR Molding Compound

 

Subcategory: Acrylic; Thermoplastic

Material Notes:
Description: PLEXIGLAS® zk4BR, PLEXIGLAS® zk5BR and PLEXIGLAS® zk6BR are impact-modified molding compounds based on polymethyl methacrylate (PMMA). The grades of the zkBR series are the most widely used impact-modified PLEXIGLAS® molding compounds. They are characterized in particular by the following properties:

  • high break resistance and impact strength
  • improved crazing resistance
  • excellent weatherability
  • brilliant optics
  • high surface hardness and abrasion resistance
  • AMECA listing

PLEXIGLAS® zk molding compounds of the BR series are suitable for extrusion and coextrusion of panels and profiles as well as for injection molding. Uses of PLEXIGLAS® zkBR molding compounds: extruded and injection-molded lighting fixture covers, extruded hollow bodies, writing utensils such as templates and fountain pens, housings, coextruded profiles for window frames, gutters, downspouts, etc., and housewares such as cutlery handles, bowls, cookie jars.

Information provided by degussa.

Available Properties
  • Density
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Melt Flow
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Charpy Impact Unnotched
  • CTE, linear 20°C
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Glass Temperature
  • Flammability, UL94
  • Refractive Index
  • Haze
  • Transmission, Visible
  • Processing Temperature
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  • Fire Rating
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。