Degussa AG Vestodur® X9405 30% Glass Reinforced, Self Extinguishing PBT

 

Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic; Polymer

Material Notes:
Description: Degussa AG’s High Performance Polymers Business Unit manufactures a range of polybutylene terephthalate compounds that are supplied under the registered trademark VESTODUR® . Material properties characterizing VESTODUR compounds are:

  • high thermostability
  • high stiffness
  • low water absorption resulting in high dimensional stability
  • high hardness
  • good strength
  • good sliding friction behavior, low abrasion
  • good creep behavior
  • good electrical properties
  • good chemical resistance
  • good weathering resistance
  • good processability
  • no tendency to form stress cracks

Specific Notes for this Material: Special types for different selective applications in the electrical, automotive, cable manufacturing, machine-building, and apparatus-construction industries. To some extent, the designations are synonyms for various product developments. Radiation crosslinkable, solder-bath resistant following radiation crosslinking.

Information provided by degussa.

Available Properties
  • Density
  • Water Absorption at Saturation
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Hardness, Shore D
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Charpy Impact Unnotched
  • Charpy Impact, Notched, Low Temp
  • Charpy Impact, Unnotched Low Temp
  • Charpy Impact, Notched
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dielectric Strength
  • Dissipation Factor
  • Dissipation Factor, Low Frequency
  • Comparative Tracking Index
  • CTE, linear 20°C
  • Melting Point
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Flammability, UL94
  • Glow Wire Test
  • Color
  • Electrolytic Corrosion
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。