Degussa AG Vestodur® X9406 Black E70167 Impact Modified PBT

 

Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic

Material Notes:
Description: VESTODUR X9406 is an impact modified compound based on polybutylene terephthalate. The resin is used as a barrier layer resin in multilayer tubing 1000.1 (MLT 1000.1)developed by Degussa. MLT 1000.1 is a 3-layer-tubing comprising an outermost layer of VESTAMID LX9010, an adhesive layer of VESTODUR X9407, and an innermost layer of VESTODUR X9406. This MLT was developed as fuel line tubing with outstanding resistance against hydrocarbon permeation when alcohol containing fuels are used. VESTODUR X9406 provides excellent barrier properties also in contact with fuels at elevated temperatures.

Information provided by degussa.

Available Properties
  • Density
  • Water Absorption at Saturation
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Charpy Impact Unnotched
  • Charpy Impact, Notched, Low Temp
  • Charpy Impact, Unnotched Low Temp
  • Charpy Impact, Notched
  • CTE, linear 20°C
  • CTE, linear 20°C Transverse to Flow
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。