Industrial Laminates/Norplex NP514MG Glass Fabric

 

Subcategory: Glass; Phenolic; Glass Fiber; Thermoset

Key Words: Micarta

Material Notes:
Description: NP514MG is made with a woven glass fabric in combination with high temperature, conductive, phenolic resin system.NP514MG has excellent flexural, compressive and impact strengths at room temperature and elevated temperatures. It was developed for the motor generator industry to provide conductive coupling to eliminate static discharges caused by corona. It is capable of continuous operation exceeding 300°C.NP514MG has excellent creep resistance because of the phenolic resin system.

Thickness Tested: 0.062”, 0.125”, and 0.500”

Information provided by Industrial Laminates/Norplex.

Available Properties
  • Specific Gravity
  • Moisture Absorption at Equilibrium
  • Hardness, Rockwell M
  • Tensile Strength, Yield
  • Flexural Modulus
  • Flexural Strength
  • Compressive Strength
  • Shear Strength
  • Izod Impact, Notched
  • Maximum Service Temperature, Air
  • Flammability, UL94
  • Bond Strength
  • Conductivity Range Surface
  • Degradation Temperature
  • Glass Transition Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。