Keysor-Century KC1252 Rigid PVC Extrusion Blow Molding Compound

 

Subcategory: Vinyl; Thermoplastic

Close Analogs:

Keysor-Century Corporation is no longer in business.

Material Notes:
A food grade extrusion blow molding compound with an excellent combination of properties for high gloss and clarity, high impact strength, low gel, and low odor. KC1252 is formulated with an FDA-approved tin stabilizer to meet the 21CFR 178.2650 food additive regulation, and is produced under stringent manufacturing conditions limiting RVCM to minimum allowable levels. Its excellent dynamic thermal stability enables easy processability with a wide variety of equipment and conditions. This permits extended production runs with minimum maintenance and downtime, and maximum regrind recycling. It is available in clear, with various levels of blue tint as free flowing pellets.

Recommended for product packages requiring compliance with FDA additive regulations to containerize liquor, edible oils, mouthwash, dry foods, and cosmetics.

Property values are typical values. Information provided by Keysor-Century Corporation.

Available Properties
  • Density
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Modulus of Elasticity
  • Flexural Modulus
  • Flexural Yield Strength
  • Izod Impact, Notched
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Transmission, Visible
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。