KiON CERASET® POLYSILAZANE 20 Heat and UV Cureable Ceramic Precursor

 

Subcategory: Thermoset; Polymer

Material Notes:
General Description

KiON Ceraset Polysilazane 20 is a liquid polymer that is readily thermoset to a solid by heating to 180-200°C. Cure can be effected at lower temperatures through the addition of a small quantity of a free radical generator. KiON Ceraset Polysilazane 20 can also be cured at room temperature by exposure to UV radiation in the presence of a UV sensitizer. The resulting solid can then be pyrolyzed to either silicon carbide or silicon nitride-containing ceramics by heating to 1,000°C. KiON Ceraset Polysilazane 20 has a higher ceramic yield than KiON Ceraset Polyureasilazane due to the elimination of low molecular weight Polysilazane components.

Applications

Ceramic Matrix Composites (CMC’s), Metal Matrix Composites (MMC’s), Ceramic MEMS, Ceramic Joining, SiC/Si3N4 coatings for C/C composites and ceramic nanocomposites.

Information provided by KiON Corporation

Available Properties
  • Density
  • Viscosity
  • Refractive Index
  • %Resin
  • Appearance
  • Graffiti Resistance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。