MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

KiON ANTI-GRAFFITI CLEAR COAT Ambient Cure, Polysilizane Clear Coat

 

Subcategory: Thermoset; Polymer

Material Notes:
General Description

KiON Anti-Graffiti Clear Coat is a clear, ready-to-use Polysilazane clear coat that can be used to resist graffiti, road tar, tree sap, dirt, grease, stains and the like. KiON Anti-Graffiti Clear Coat will cure at ambient temperature and is dry-to-touch within 1 hour of application. KiON Anti-Graffiti Clear Coat can easily be applied by spraying, dipping, or brush coating. Resistance to most graffiti insults (permanent marker, etc.) can be obtained after a two day cure and full anti-graffiti protection against spray paint can be obtained after a 7 day cure. Dried spray paint can be removed from surfaces coated with KiON Anti-Graffiti Clear Coat by mild mechanical abrasion or spray washing. In addition, KiON Anti-Graffiti Clear Coat has excellent “weatherability”, UV resistance, hardness, and abrasion resistance, as well as oxidation and corrosion resistance.

Applications

Suggested major applications include but are not limited to transportation, highway signage, and building facades.

Information provided by KiON Corporation

Available Properties
  • Density
  • Volatile Organic Compounds (VOC) Content
  • Flash Point
  • %Resin
  • Adhesion ASTM D 3359
  • Appearance
  • Chemical Resistance
  • Pencil Hardness ASTM D 3363
  • UV Stability
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。