KKPC KOSYN 1500NF Styrene Butadiene Rubber

 

Subcategory: Styrene-Butadiene; Elastomer, TS; Thermoset

Material Notes:
Styrene Butadiene Rubber

Characteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and heat resistance in comparison with natural rubber, as well as widely useful physical properties of easy vulcanization and stable scorch properties. The products of KOSYN SBR are classified according to the emulsifying agent and stabilizer used in manufacturing process.

Applications: Tires, footwear, rubber hose, auto equipment and other rubber products for industrial use.

Additional Notes:
Bound Styrene: 23.5%
Stabilizer: Staining
Emulsifier: Rosin soap
Coagulant: Salt-Acid
Compound Properties: SRB 100, ZnO 3, S/A 1, HAF Black (IRB#7) 50, Accelerator TBBS1, Sulfur 1.75, Total: 156.75
Vulcanization: 145°C *35 m., Press Vulcanization

This product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants.

Data provided by Korea Kumho Petrochemical Co., Ltd.

Available Properties
  • Density
  • Mooney Viscosity
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • 300% Modulus
  • Rebound
  • Flex Crack Resistance
  • Tear Strength
  • Abrasion
  • Compression Set, Elevated Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。