MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Kydex® 150 Acrylic/PVC Thermoplastic Sheet

 

Subcategory: Vinyl; Acrylic; Thermoplastic

Key Words: Polyvinylchloride; PMMA; Polymethylmethacrylate

Material Notes:
Class I/A rated thermoplastic sheet

Applications: Interior ductwork and chutes, laboratory hoods, shower/tub shrouds, acoustical applications, decorative ceilings, abuse resistant surfacing for counters, exhibits, portions, doors

Features: Kydex 150 is more resistant to a wider range of concentrated chemicals than any other thermoplastic. Its superior chemical resistance allow for excellent cleanability because stronger clearing agents can be sued with no discoloration or surface damage to the material. It is not available for field applied wallcovering applications. Flammability Properties: Flame Spread at 25 minutes. Fire Door at 20 minutes (ASTM E152).

Fabrication: Kydex 150 has good formability and extensibility and is extremely easy to work with once formed. All secondary operations, such as sawing, shearing, punching, and brake forming are possible with Kydex 150 sheet.

Data provided by the Kleerdex Company.

Available Properties
  • Density
  • Hardness, Rockwell R
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Modulus of Elasticity
  • Flexural Yield Strength
  • Izod Impact, Notched
  • Taber Abrasion, mg/1000 Cycles
  • Deflection Temperature at 1.8 MPa (264 psi)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。