Invista 1101 PET Copolymer Packaging Resin

 

Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic; Polymer

Key Words: Excellent melt and crystallization properties

Material Notes:
Carboxyl end groups: <30 meg/kg.
Diethylene glycol content: <1.8 wt%.
Acetaldehyde content: <2.0 ppm.
Fines 0.1% through 28 mesh as manufactured.
Moisture content <0.1% as manufactured.
Chip size <1.8±0.3mm avg. dia. flat side.
Crystallinity >50%.

1101 PET is a copolymer packaging resin with a nominal intrinsic viscosity of 0.84 dl/g. 1101 resin has excellent melt and crystallization properties, offering easy processibility in injection molding and stretch-blow molding.

Packaging made from this resin has excellent clarity and is noted for its dimensional stability, which prevents shrinkage and expansion of the container. It conforms to FDA Regulation 177.1630 for food contact and is widely used for single-serve beverage bottles, small liquor bottles, and other custom containers. Containers made from PET are light weight, have excellent clarity, are recyclable, and are shatterproof.

Information supplied by the manufacturer.

Available Properties
  • Density
  • Apparent Bulk Density
  • Viscosity Measurement
  • Melting Point
  • Process
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。