Lendell Manufacturing Prepol Pre Polymers

 

Subcategory: Polyurethane, TS; Thermoset

Material Notes:
Liquid Apperance, Amber, honey like

Polyether Polyurethane Pre-Polymer is water activated, yielding foams and gels with unique characteristics - Hydrophilic, Bio-Compatible, loading of additives to 80% by weight and a very low exotherm reaction.

Applications:

Cosmetic, Consumer Products, Filtering, Medical, Agricultural, Wicking, Thermal, Acoustical, Wiping, Industrial, Insulations, Fire Protection, Sports/Leisure, Cushioning, Flotation, Automotive, Anti-Static, Toys

Foam Additives:

Colors, Fragrances, All Liquids, Solids, Abrasives, Microbicides - Live Algae

Information provided by Lendell Manufacturing Inc.

Available Properties
  • Density
  • Viscosity
  • Flash Point
  • Melt Temperature
  • % Free Toulene Diisocyanate
  • % NCO content
  • Equivalent Wt (per NCO)
  • NCO (meq/g)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。