Plenco VALITE 759 Novolac Phenolic, Granular, Injection Molded

 

Subcategory: Phenolic; Thermoset

Close Analogs:
Plenco has discontinued their Valite product line.

Material Notes:
This Valite product has been replaced by Plenco 4759. Data provided by Plenco.

VALITE 759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and possesses good electrical properties. It is used in applicance and electrical applications and can be molded by compression, transfer, or injection processes. It is UL recognized under component file E59891. VALITE 759 is the same formulation as PLENCO 04759. Plenco drop ball 113g test value is 34 cm.

Available Properties
  • Density
  • Apparent Bulk Density
  • Water Absorption
  • Linear Mold Shrinkage
  • Hardness, Rockwell E
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Yield Strength
  • Compressive Yield Strength
  • Izod Impact, Notched
  • Charpy Impact, Notched
  • Electrical Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Arc Resistance
  • Comparative Tracking Index
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。