Loctite® U-10FL Plastic bonder, highly flexible, high peel Durabond® Urethane Adhesive

 

Subcategory: Adhesive; Polyurethane, TS; Thermoset

Material Notes:

Urethane Adhesives
Loctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 application-specific products designed to outperform the competition in all aspects: better adhesion, better flow, less odor, improved clarity, higher strength, and greater durability. All two-part Durabond® Structural Adhesives are packaged in easy-to-use, side-by-side cartridges for use with our manual dispensers and mix nozzles.

Loctite® U-10FL Plastic bonder, highly flexible, high peel Durabond® Urethane Adhesive
A two-part, high-performance urethane adhesive for plastic bonding with a 10-minute worklife. Ultra-clear, highly flexible, impact resistant, high peel.

  • Mix Ratio by Volume, Resin:Hardener = 1:1
Bonding Type: Urethane

Available Properties
  • Viscosity
  • Hardness, Shore D
  • Shear Strength
  • Peel Strength
  • Dielectric Strength
  • Glass Temperature
  • Pot Life
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。