Loctite® 444 General Purpose Ethyl Tak Pak™ Instant Adhesive

 

Subcategory: Adhesive; Thermoset; Cyanoacrylate

Material Notes:

Cyanoacrylate Bonding Adhesives and Gasketing and Wire Tackers
Loctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-specific, instant adhesives. Loctite® Instant Adhesives are available in a variety of viscosities, cure speeds, gap-filling capability and substrate compatibility. The ultra high-performance PRISM® family offers additional products that surpass the most stringent demands, including toughened formulations, low odor and low blooming products, surface insensitive and thermally resistant formulations.

Loctite® innovative gasketing products offer precise, reliable sealing of electronic enclosures, protecting them from environmental hazards. Loctite offers both Form-in-place (FIP) and Cure-in-Place (CIP) compression gasket materials.

Loctite® Tak Pak Adhesives are used to secure wires to printed circuit board assemblies. The fast cure times of these adhesives help increase the throughput of the wire tacking assembly process.

Loctite® 444 General Purpose Ethyl Tak Pak™ Instant Adhesive
An adhesive designed for printed circuit board assembly and repair. Cures instantly with Tak Pak® Accelerator. Used to tack jumper wires and wires to coil forms. Tamper-proof adjustable components. Mounting standoffs, edge guides and stiffeners to circuit boards. Cure Type: Accelerator Bonding Type: Ethyl cyanoacrylate Commercial item std. A-A-3097 Type II, Class 3 Typical Use: Tak Pak® Wire tacking adhesive

Available Properties
  • Density
  • Viscosity
  • Shear Strength
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Color
  • Gap Fill
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。