Meilian Chemical Co. BLACK MASTERBATCH PE-B1301

 

Subcategory: Polyethylene; Thermoplastic; LDPE

Material Notes:
BLACK PE-B1301 is a black low density polyethylene based masterbatch containing pure high opacity carbon black. It is designed for use in high jet black film with excellent surface performance, such as high opacity mulch. It also can provide premium tinting strength for Injection Molding items and Hollow Blown Films.

Method of Usage: BLACK PE-B1301 is designed for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resin mixer, avoiding pollution and malscattering problems caused by pigment.

Range of Application: BLACK PE-B1301 is designed for use in LDPE, HDPE, LLDPE and PP.

Available Properties
  • Density
  • Melt Index of Compound
  • Carrier
  • Compatibility
  • Pigment Content: Carbon Black (%)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。