MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Merquinsa Pearlthane® D11T93 Polycaprolactone Copolyester based TPU

 

Subcategory: Polyurethane, TP; Thermoplastic

Material Notes:
Pearlthane® 11 series is based on Merquinsa`s proprietary polycaprolactone (PCL) technology. It offers a unique combination of key benefits vs. standard TPU polyesters:

  • Significant lower part cost because of intrinsic lower density and faster processing
  • Superior performance such as hydrolysis resistance, abrasion resistance and low temperature impact properties.

Very fast cycling injection moulding grade offering easy mould release, lower density and abrasion resistance.

Applications: Automotive parts, animal ID tags, gasket & seals, mining screens, snow parts, casual and sport shoe soles, shoe heels, engineering parts, and overmoulding.

The values shown are typical values and should not be used for establishing specifications.

Available Properties
  • Density
  • Melt Index of Compound
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • 100% Modulus
  • 300% Modulus
  • Abrasion
  • Compression Set
  • Transformation Temperature, Tg
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。