Metton M1534 - M1540 LMR Liquid Molding Resins

 

Subcategory: Thermoset

Key Words: Metton LMR

Material Notes:
Different product numbers represent different formulations for customer specific needs such as liquid freezing point. Metton LMR is a tough and durable engineering plastic material used to produce large or thick molded parts for many diversified applications. The Metton LMR reaction injection molding process can provide large parts in low pressure molds with the mechanical property performance similar to injection molded engineering thermoplastics. The combination of Metton LMR’s process and material capabilities result in a new design freedom for replacing traditional materials such as metal, wood and fiberglass.

Injection molded engineering thermoplastics have a similar benefit package for smaller parts. Small parts for Metton LMR are in the 8 to 10 ft² (1 m²) range which is the upper end for cost and size capability for standard injection molding. In addition, Metton LMR parts do not require identical part geometry for multi-cavity molds.

Metton LMR is a family of lightly cross linked olefinic thermoset polymers based on polydicyclopentadiene (PDCPD) with mechanical property performance attributes similar to engineering thermoplastics. In the Metton LMR molding process, two low - viscosity DCPD liquid streams - one containing an activator (A Component) and the other a catalyst (B Component) - are impingement mixed at a 1:1 ratio and injected at near room temperature into a closed mold. The resulting exothermic reaction (heat generating) creates a fully polymerized part in less than 60 seconds. Button to button cycle times are generally 4 to 6 minutes depending upon size and geometry

Available Properties
  • Density
  • Water Absorption
  • Linear Mold Shrinkage
  • Hardness, Rockwell R
  • Tensile Strength, Yield
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Yield Strength
  • Compressive Yield Strength
  • Poissons Ratio
  • Shear Strength
  • Izod Impact, Notched
  • Izod Impact, Notched, Low Temp
  • CTE, linear 20°C
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Glass Temperature
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。