Mitsui AURUM® JCF3030 Polyimide, Carbon Fiber/PTFE Filled

 

Subcategory: Polyimide; Thermoplastic; Polymer

Material Notes:
AURUM JCF3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AURUM JCF3030 offers a unique balance of mechanical, thermal, and tribological properties for outstanding performance in demanding automotive, business machinery, industrial equipment, aerospace, and semiconductor equipment applications. AURUM components offer excellent mechanical strength and toughness, dimensional stability, low outgassing, and exceptional radiation resistance. In addition, AURUM exhibits outstanding resistance to hydraulic, automotive, and many industrial fluids and solvents, a low coefficient of thermal expansion, creep resistance, and flame retardancy. AURUM JCF3030 withstands high PV levels and provides a low wear factor and low friction surface over a broad temperature range in lubricated environments.

Applications: AURUM JCF3030 components are excellent replacements for metals, ceramics, and other plastics. High performance AURUM parts include: thrust washers and oil seal rings for automotive and off road vehicle transmissions, thermal insulators and stripper fingers for high-speed copiers, jet engine components, check valve balls, spline couplings, heat-resistant gears, vanes, wear strips, and valve seats. Other AURUM applications include carriers for aluminum hard disks and silicon wafers, journal bearings, and bearing retainers.

Information provided by DuPont

Available Properties
  • Specific Gravity
  • Water Absorption
  • Moisture Absorption at Equilibrium
  • Linear Mold Shrinkage, Transverse
  • Melt Flow
  • Tensile Strength, Yield
  • Elongation at Yield
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • Melting Point
  • Transformation Temperature, Tg
  • Deflection Temperature at 0.46 MPa (66 psi)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。