Montell Adstif KC-732P LTHA Thermoplastic Olefinic Copolymer

 

Subcategory: Thermoplastic

Close Analogs:

Basell is the successor company to Montell.

Material Notes:

Key Features: LTHA thermoplastic olefin copolymer resin for injection molding applications, excellent heat resistance, high stiffness and gloss, good weld line strength, good creep resistance

Applications: appliance parts, automotive parts, power tools, lawn and garden

All ingredients meet TSCA (US) and DSL (Canada) registration requirements.

Description: Adstif KC-732P polyolefin copolymer resin is designed for long term heat aging injection molding applications. This resin is highly resistant to long term heat again in both wet and dry environments. It is based on material produced from Montell's proprietary Catalloy process. This resin offers a unique balance of properties: high stiffness, impact resistance heat performance and good processability. It has a UL flame class rating of 94HB that applies to all colors. All ingredients meet the chemical registration requirements of TSCA and DSL.

Information provided by Montell Polyolefins.

Available Properties
  • Density
  • Melt Flow
  • Hardness, Rockwell R
  • Tensile Strength, Yield
  • Elongation at Yield
  • Flexural Modulus
  • Izod Impact, Notched
  • Deflection Temperature at 0.46 MPa (66 psi)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。