Montell Hifax CA186 Thermoplastic Olefin Resin

 

Subcategory: Thermoplastic

Close Analogs:

Basell is the successor company to Montell.

Material Notes:

Key Features: medium melt flow, medium modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, excellent paintability and paint durability, good processability, colorable

Applications: fully painted and selectively decorated automotive bumper fascias, molded-color exterior components

Description: Hifax CA186 medium melt flow, reactor grade thermoplastic elastomeric olefin resin has an ecellent balance of impact, stiffnss and apintability. It is based on material produced from Montell's proprietary Catalloy process and was designed primarily for painted automotive bumper fascias that require high durability.

Information provided by Montell Polyolefins.

Available Properties
  • Density
  • Linear Mold Shrinkage
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Flexural Modulus
  • Izod Impact, Notched, Low Temp
  • Impact Test
  • CTE, linear 20°C
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。