Montell Polybutene-1 DP 8310

 

Subcategory: Polybutene; Thermoplastic

Close Analogs:

Basell is the successor company to Montell.

Material Notes:

Key Features: semi-crystalline high ethylene content random copolymer

Applications: packaging industry, cast film, FDA acceptable

Meets FDA requirements in 21 CFR 177.1570 for direct food contact up to 212°F (100°C).

Description: Polybutene-1 DP 8310 is a semi-crystalline high ethylene content random copolymer which is miscible with polypropylenes due to its similar moecular structure. In blends with polyethylene it is immiscible but easily dispersible. It is used in the packaging industry as a minor additive in a polyethylene peel seal layer for the production of coextruded glexible film or more rigid sheet. Varying the copolymer concentration in th peel seal layer offers the unique possibility of tailoring the seal strength blown or cast film formulations when imporved optical properties of the reulting fim are required. A typical blend partner is a low density polyethylene iwth a melt index range between 0.5 and 4 dg/min. All other polyethylene types and copolymers of the same melt index range can be used. It can also be used in blends wiht polypropylenes to reduce flexural modulus and hardness characteristics very effectively. This resin meets FDA requirements for direct food contact at temperatures up to 100°C under regulation 21 CFR 177.1570.

Information provided by Montell Polyolefins.

Available Properties
  • Density
  • Melt Flow
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Melting Point
  • Vicat Softening Point
  • Brittleness Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。