Basell Adflex™ Z104S Thermoplastic Polyolefin Elastomer

 

Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic; Polymer

Material Notes:
Description: Adflex™ Z104S, a versatile thermoplastic olefin resin, can be used for injection molding, impact modification, extrusion coating or film and fiber applications. This resin is based on proprietary Basell technology and can be used on conventional injection molding or extrusion equipment. Z104S resin features a very high softness and low modulus, with a high melt flow. It is ideal for the modification of polypropylene without altering the transparency of the modified polypropylene (homopolymer or random copolymer). It meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.2600 for resins in rubber articles for repeated use applications. The final item is subject to the extraction tests specified in 21 CFR 177.2600. All ingredients in Z 104 S resin meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Household goods, toys

Information provided by Basell.

Available Properties
  • Density
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Flexural Modulus
  • Izod Impact, Notched
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。