Custom Resins Nylene® 474 Nylon 6

 

Subcategory: Nylon; Thermoplastic; Nylon 6

Close Analogs:

Data provided by the manufacturer

Key Words: Polyamide 6

Material Notes:
Dry as molded. Nylene 474, for rotational molding, is offered in small pellet form which helps overcome the moisture problems associated with powdered nylons. All Custom Resins nylons are dried to less than 0.1% moisture eliminating the need for predrying of virgin material. Nylene 474 is molded with wall thicknesses ranging from 1/16" to greater than 1". Rotational molding of Nylene 474 is processed in ovens heated to 575 - 700ºF. Temperatures below 700ºF are preferred. We strongly recommend the use of inert gases such as nitrogen in the mold to prevent thermal degradation of the nylon.

Available Properties
  • Density
  • Water Absorption
  • Elongation at Break
  • Izod Impact, Notched
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。