Nycoa® 2084 HS Super-Tough, High Viscosity Nylon 6 Resin

 

Subcategory: Nylon; Thermoplastic; Nylon 6

Material Notes:
NYCOA 2084 HS is a high viscosity resin particularly suitable for extrusion processing. Its melt viscosity and strength provide ease of processing for tubing, profile, and molded articles.

This material has been specially formulated with an organic heat stabilizer to eliminate copper iodide extraction in windshield-wiper tubing applications. In addition, the base resin in fully extracted to minimize caprolactam extractables.

Typical applications include automotive tubing, windshield washer tubing, and hoses.

Information provided by Nycoa, Inc.

Available Properties
  • Specific Gravity
  • Water Absorption
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。