MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Omnia Plastica - Acetal Copolymer - POM c

 

Subcategory: Acetal; Thermoplastic

Material Notes:
Polyoxymethylene, commonly called Acetal, is a crystalline polymer obtained from the polymerisation of formaldehyde. Discovered fairly recently (1960), it has enjoyed rapid growth and large acceptance thanks to it’s excellent mechanical features, stability to humidity and ease of machining. All our stock shapes made of POM are marked along the whole length with product code and batch number, according to ISO 9002 standards.

Features:

  • High fatigue resistance
  • Good dimensional stability
  • Low friction coefficient
  • Compressive strength, shock resistance, even at low temperature
  • Excellent machinability especially used on automatic equipment
  • Colour: natural and black
Weak Point:

Compared to PA6 it has a lower abrasion resistance, particularly in dirty and dusty environments.

Application:

  • Mechanical: it is one of the most commonly used engineering plastics for mechanical applications such as bearings, cams, gears with low torque, gear wheels, conveyor rollers and precision machined components requiring dimensional stability and tight tolerances.
  • Food contact: being physiologically inert it is suitable for food contact. It can be used in water at 80° C.
  • Electrical: as it is not hygroscopic, it is commonly used for electric components such as insulators.
  • Chemical: it is resistant to alkali and organic compounds. Thanks to its good chemical properties it is suitable for pump components, flanges and components for chemical plants.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Available Properties
  • Density
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Hardness, Rockwell M
  • Ball Indentation Hardness
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Compressive Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Coefficient of Friction
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Oxygen Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。