Omnia Plastica - Acetal Homopolymer - POM h

 

Subcategory: Acetal; Thermoplastic

Material Notes:
The general features of homopolymer acetalic resin are similar to those of copolymer POM c, except that service temperature (under load) is slightly higher but resistance to hydrolysis and strong alkali is lower.

Features:

  • High fatigue resistance.
  • Good dimensional stability.
  • Low friction coefficient High compressive strength.
  • The shock resistance is good even at low temperature.
  • Excellent machinability, especially on automatic equipment
  • Colour: natural
Weak Point:

Compared to PA6 it has lower abrasion resistance, particularly in dirty and dusty environments. Compared to POM c. its resistance to hydrolysis is lower.

Application:

  • Mechanical: it is used for mechanical applications such as bearings, cams, gears with low torque, gear wheels, conveyor rollers and dimensionally stable precision parts.
  • Food contact: being physiologically inert, it is suitable for food contact. It can be used in water at 80° C.
  • Electrical: as it is not hygroscopic, it is commonly used for electric components such as insulators.
  • Chemical: it is resistant to alkali and organic compounds. Thanks to its good chemical properties it is suitable for pump components, flanges and components for chemical plants.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Available Properties
  • Density
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Hardness, Rockwell M
  • Ball Indentation Hardness
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Compressive Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Coefficient of Friction
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Oxygen Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。