Omnia Plastica - Akulon GX - PA 66.6 Dry

 

Subcategory: Nylon; Thermoplastic; Nylon 6/66

Material Notes:
Copolymer of nylon with excellent mechanical features, it combines the good impact resistances of PA6 as well as the higher stiffness of PA66. For this reason it machines very well on automatic tools and on CNC centres. The U.V. stabilisation makes it light resistant and it is therefore suitable for outdoor applications.

Features:

  • Wear resistance: good even in demanding environments. Toughness: high tensile stress and compressive strength.
  • Self-lubricating: the friction coefficient is low and generally for sliding application it does not require lubricators.
  • U.V. resistance: particularly suitable for outdoor applications it withstands atmospheric agents and low temperatures very well.
  • Machining on automatic tools is easy thanks to the breaking of shavings during machining and to its higher stiffness.
  • Black colour.
Weak Point:

It is hygroscopic (even if at lower extent than PA6) therefore the mechanical features and the dimensions will change consequently

Application:

  • Mechanical: thanks to its higher stiffness compared to PA6 and its higher shock resistance compared to PA66, this material is increasingly being used in the mechanical field to produce gears, cams, pulleys, anti-wear guides, wheels and other components, notably for outdoor use. In the field of construction and earthmoving equipment Akulon GX can be found in guides, bearings and pulleys. it is particularly suitable for machining on automatic lathes.
  • Food contact: generally it is not used in contact with food.
  • Electrical: use in the electrical field is to be avoided as the electrical features change with the moisture content. It is sometimes used when its mechanical features are required.
  • Chemical: it is resistant to alkali, inorganic compounds and solvents.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Available Properties
  • Density
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Hardness, Rockwell M
  • Ball Indentation Hardness
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Compressive Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Coefficient of Friction
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Oxygen Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。