Omnia Plastica - Akulon 66 - PA 66 Dry

 

Subcategory: Nylon; Thermoplastic; Nylon 66

Material Notes:
Polyamide obtained by the polymerisation of Hexamethylenediamine and Adipic acid. It is one of the oldest engineering plastics, having been created in the USA in 1930. Due to its origin it is widely used in the American and English markets. In comparison to PA6 it is more stiff and tougher but is also more brittle. It is advisable to use PA66 instead of Polyamide 6 when a higher stiffness is required to the detriment of resilience. It can be easily machined on automatic machine tools. All our stock shapes made of PA 66 are marked along the whole length with product code and batch number, according to ISO 9002 standards.

Features:

  • Wear resistance: it is good even in demanding environments.
  • Self-lubricating: the friction coefficient is low and generally for sliding application it does not require lubricators.
  • Toughness: very high tensile stress and compressive strength. Its toughness is higher than that of Polyamide 6.
  • Machining on automatic machine tools is shown to be easy as the shavings break thanks to its higher toughness.
  • Ageing resistance and weatherproof.
  • Natural colour.

Weak Point:

It is hygroscopic, even if to a lesser extent than PA6. It absorbs moisture in time and consequently the mechanical features and the final dimensions will change.

Application:

  • Mechanical: because it has a higher stiffness than PA6 it is used for mechanical applications when this feature is more important than that of shock resistance: suitable for gears, cams, pulleys, anti-wear guides, wheels and mechanical parts. Like Akulon GX, it machines very easily on automatic tools.
  • Food contact: in some cases it can be used in contact with food.
  • Electrical: use in the electrical field is to be avoided as the electrical features change with the moisture content.
  • Chemical: it is resistant to alkali, inorganic compounds and solvents.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Available Properties
  • Density
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Hardness, Rockwell M
  • Ball Indentation Hardness
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Compressive Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Coefficient of Friction
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Oxygen Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。