MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Omnia Plastica - Rilsan B - PA 11

 

Subcategory: Nylon; Thermoplastic; Nylon 11

Material Notes:
The only engineering plastic of natural origin (derived from castor oil), it is a polyamide which, unlike the other nylons, does not absorb humidity. It has all the good mechanical features of polyamides: tensile stress, compressive strength, wear resistance, etc. Moisture content does not influence its shock resistance. It has very good ageing and low temperature resistance.

Features:

  • Tensile stress, compressive strength and shock resistance values stable in moist as well as dry environments Wear resistance: very good even in dusty or demanding environments.
  • Ageing and low temperature resistance Self-lubricating; low friction coefficient.
  • Generally for sliding applications it does not require lubricators.
  • Colour: natural.
Weak Point:

Although Nylon 11 has all the excellent mechanical features of polyamides without their weakest point (hygroscopicity), its high price prevents wider usage.

Application:

  • Mechanical: thanks to the stability of its excellent mechanical features, both in moist environments and at low temperatures, it is used especially in aeronautic, marine, and transport applications, and in machinery as bushings, bearings, slide and mechanical parts.
  • Food contact: it is physiologically inert and it is used in food processing machinery.
  • Electrical: as it is not hygroscopic and its electrical properties are stable, it is widely used for electrical applications such as insulators.
  • Chemical: it is resistant to solvents.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Available Properties
  • Density
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Hardness, Rockwell M
  • Ball Indentation Hardness
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Compressive Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Coefficient of Friction
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Oxygen Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。