Omnia Plastica - Polysulphone - PSU

 

Subcategory: Polysulfone; Thermoplastic

Material Notes:
It is a non-reinforced amorphous polymer whose main features are its high thermal, electrical and mechanical properties which are typical of a crystalline polymer. Compared to its "brother" PES it has lower thermal properties, although this level is still high when compared to most other engineering plastics.

Features:

  • Resistance to high temperature.
  • Resistance to hydrolysis and steam.
  • Mechanical properties : tensile stress, flexural strength, E.modulus
  • Chemical resistance
  • Electrical properties
  • Transparency
Weak Point:

The cost is higher than conventional engineering plastics. It does not stand UV rays and is therefore not suitable for outdoor applications.

Application:

  • Electrical: the very good insulating and dielectric properties make it irreplaceable in many electrical applications: plates for circuits, coils, insulators.
  • Mechanical: it is used for high performance applications such as bearings and precision gears at low as well as high temperatures.
  • Chemical: the use in this field is ideal thanks to its high chemical and thermal resistance. Good resistance to mineral acids, alkali and salt solutions. PSU is attacked by esters, chlorine and aromatic hydrocarbons.
  • Food contact: it is physiologically inert and is therefore used for parts in contact with food, even at high temperature. The excellent chemical properties make it suitable for pump components, flanges, etc. which are in contact with food liquids.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Available Properties
  • Density
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Hardness, Rockwell M
  • Ball Indentation Hardness
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Compressive Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Coefficient of Friction
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Oxygen Index
  • Form
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。