Omnia Plastica - Polypropylene - PP

 

Subcategory: Polypropylene; Thermoplastic

Material Notes:
The mechanical features of PP are better than those of PE H.D. It withstands attack by alkali and acids and consequently it is widely used for components in the chemical industry when a moderate stress material is required.

Features:

  • Chemical: high chemical resistance.
  • Tensile stress: very high among the polyolefins.
  • Low specific gravity.
  • Easy machinability on mechanical tools. It can be welded.
  • Good stability to temperature.
  • Colour: grey RAL 7032 and natural
Weak Point:

Compared to the engineering plastics it has low thermal and mechanical properties: tensile stress, flexural and compressive strength, etc. Compared to PE it is more rigid but less shock resistant.

Application:

  • Chemical: the widest application field for PP is the chemical industry. Thanks to its high resistance to acids and alkali and its higher temperature resistance than PVC, it is used for components in the chemical, galvanic and petrochemical industries to produce valves, flanges, gears, etc.
  • Food contact: it is physiologically inert, so in natural form, it is approved for use in contact with food.
  • Electrical: good dielectric properties. Weather stability is its best feature for this application.
  • Mechanical: it is also used for mechanical components in corrosive environments. It has a higher tensile stress than H.M.W. PE.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Available Properties
  • Density
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Hardness, Rockwell R
  • Ball Indentation Hardness
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Compressive Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Coefficient of Friction
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Oxygen Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。