Omnia Plastica - Polyetheretherketone - PEEK

 

Subcategory: Polyketone; Polyetheretherketone (PEEK); Thermoplastic

Material Notes:
Semicrystalline polymer. Material with high mechanical and thermal properties (up to 240°C.). It resists to creep under load and to wear, its friction coefficient is low.The temperature resistance without load is high but it is reduced by the additon of load even if limited.

Features:

  • High temperature. It resists beyond 240°C. (The Heat distorsion temperature is 162°C)
  • Dimensional stability
  • Good chemical resistance
  • Good abrasion resistance and low friction coefficient.
  • Electrically insulation
Weak Point:
  • Very high cost.
  • Load bearing decreases above 140° C.
  • Not inherently U.V. stable.
Application:
  • Mechanical: The dimensional stability at temperature is high, as well as the heat resistance. The components obtained have a high wear resistance and are self-lubricated. It is used to high performance pieces at low as well as at high temperatures:gears bushes, in aircraft and aerospace industries.
  • Electrical: Very good dielectric and insulating properties.
  • Chemical: Very good chemical resistance. Ball valve seals, pump housings
  • Nuclear: High resistance to gamma radiation

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Available Properties
  • Density
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Hardness, Rockwell M
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Oxygen Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。