Petromont HDPE 7001

 

Subcategory: Polyethylene; Thermoplastic; MDPE; Polymer

Key Words: Geomembrane, pond liners-sheet

Material Notes:
Petromont HDPE 7001 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is designed to be readily processed by flat die extrusion equipment.

Petromont HDPE 7001 is an unpigmented polyethylene compound which, after proper incorporation of carbon black, may be used for geomembrane applications, such as liners for landfills and surface impoundments, where polyethylene is the material of choice. Comprehensive information on such facilities is available in documents issued by the U.S.A EPA.

Available Properties
  • Density
  • ESCR 100% Igepal®
  • Oxidative Induction Time (OIT)
  • Melt Flow
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Modulus
  • Process
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。