Cookson Group Plaskon® SMT-B-1N Molding Compound for PBGAs

 

Subcategory: Epoxy; Adhesive; Thermoset

Material Notes:
This material is an epoxy molding compound optimized specifically for PBGA applications with no plasma cleaning required before molding. It has the same unique resin system as the SMT-B-1, which minimizes warpage and enables trouble-free molding onto rigid and flexible laminate substrates. Minimal dimensional change after molding, post bake and subsequent solder treatment make this compound an excellent choice for PBGA and CSP applications.

Features:

  • Faster cure speed
  • Improved wire sweep performance
  • Lower viscosity
  • No plasma cleaning required before molding

Information provided by Cookson Electronics

Available Properties
  • Specific Gravity
  • Moisture Absorption at Equilibrium
  • Viscosity
  • Spiral Flow
  • Ash
  • Storage Temperature
  • Hardness, Shore D
  • Flexural Modulus
  • Flexural Strength
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Thermal Conductivity
  • Glass Temperature
  • Flammability, UL94
  • Oxygen Index
  • Mold Temperature
  • Back Pressure
  • Cure Time
  • Cure Time
  • Gel Time
  • Shelf Life
  • Hydrolyzable Halides
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。