Cookson Group STAYCHIP® 2078E No-Flow Fluxing Underfill

 

Subcategory: Adhesive; Thermoset

Material Notes:
STAYCHIP 2078E no-flow underfill is used to perform the dual functions of a solder flux and an underfill between (1) a flip chip die and a substrate or (2) an area array device and a printed circuit board. This material functions as a flux as it solders Sn63/Pb37 bumped pads to common pad metallizations (eutectic Sn/Pb, Cu/Ni/Ag, and OSP coated Cu), using a conventional reflow profile. The product also functions as an underfill as it cures during the conventional reflow profile, immediately after soldering, forming a stress absorbing, compliant matrix that distributes the stress imposed by the CTE mismatch between the die and substrate. This matrix provides enhanced environmental protection and shock resistance.

Features:

  • Uses conventional reflow profile to fully cure, with no post-reflow cure needed
  • Little or no voiding when the appropriate STAYCHIP no-flow underfill product is matched to the desired reflow profile
  • Excellent wetting
  • Cure kinetics matched to common Sn63 reflow profiles for high yield process
  • Very low ionic content
  • Exceptional thermal shock/impact resistance

Information provided by Cookson Electronics

Available Properties
  • Specific Gravity
  • Moisture Absorption at Equilibrium
  • Viscosity
  • Storage Temperature
  • Hardness, Shore D
  • Dielectric Constant
  • Dissipation Factor
  • CTE, linear 20°C
  • Glass Temperature
  • Pot Life
  • Shelf Life
  • Appearance
  • Chemical Type
  • Ionic Content, Acetate
  • Ionic Content, Ca
  • Ionic Content, Cl
  • Ionic Content, K
  • Ionic Content, Na
  • Ionic Content, Nitrate
  • Storage Modulus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。