Precision Polymer Engineering Perlast® G90S White Perfluoroelastomer

 

Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset

Key Words: Rubbers

Material Notes:
Perlast ® G90S is a White Perfluoroelastomer 86-95 °IRHD with excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and formulated in accordance with United States Food and Drug Administration (FDA) requirements, Code of Federal Regulations Title 21 (CFR21), Section 177.2600. In July 2004, G70S gained Food Contact Notification status (FCN) from the FDA (FCN000402).

Applications: Approved according to FDA regulations for repeated use in equipment associated with the production of foodstuffs intended for human consumption. Do not use any Perlast ® grade with molten alkali metals.

Available Properties
  • Hardness, Shore A
  • Tensile Strength, Yield
  • Elongation at Break
  • Compression Set
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。