Precision Polymer Engineering Perlast® G75S Perfluoroelastomer

 

Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset

Key Words: Rubbers

Material Notes:
Perlast® G75S has been specifically developed to cope with a wide range of process media, potent active pharmaceutical ingredients (APIs) and aggressive cleaning agents, being especially suited to withstand steam-in-place (SIP) and clean-in-place (CIP) procedures within pipe work and vessels. G75S is also suitable for other critical applications such as Water-For-Injection (WFI) systems. Perlast® G75S is an all round material that can be used for all types of applications requiring FDA and USP Class VI compliance. It is suitable for use in all product contact applications including dry, aqueous and fatty media. Unlike other FDA compliant elastomers, Perlast® G75S is thermally stable at higher temperatures, and is ideal for use in applications which require exposure to temperatures up to 310°C (590°F) making it suitable for use in Stage II Sterilization processes. Perlast® G75S is suitable for both dynamic and static applications and can be moulded into O-rings and custom shapes.

Applications: Recommended for use in pharmaceutical, bio-analytical and food processing applications, where both mechanical and chemical properties are crucial, and hygienic sealing capability is critical. Dynamic Seals: Split butterfly valve seals; Ball segment valve seals. Static Seals: O-rings; Pressure safety rings; Gaskets; Hygienic & sanitary couplings; Mechanical seals for stirring/mixing screws & pumps

Available Properties
  • Hardness, Shore A
  • Tensile Strength, Yield
  • Elongation at Break
  • 100% Modulus
  • Compression Set
  • CTE, linear 20°C
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。