Precision Polymer Engineering S50D Silicone Rubber

 

Subcategory: Silicone; Elastomer, TS; Thermoset

Material Notes:
Black Silicone Rubber, 46-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated to meet UK Ministry of Defence Aircraft Materials Specification DTD5531A Grade 50. ASTM & ISO designation = VMQ.

Applications: Sheets, mouldings and extrusions for mainly mechanical applications in contact with air within the quoted temperature range. They are not intended for liquid sealing or for application where low compression set is of prime importance. Occasional contamination by silicate ester and phosphate ester hydraulic fluids and greases is not unduly detrimental, provided the temperature is not excessive. Contact with fuels, light mineral oils, silicone liquids or greases derived from these should be avoided. Excellent ozone resistance.

Available Properties
  • Hardness, Shore A
  • Tensile Strength, Yield
  • Elongation at Break
  • Compression Set
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Flash Point
  • Low Temperature Resistance, °C
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。