MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Premix Thermoplastics PRE-ELEC® ESD 6110

 

Subcategory: Polystyrene; Additive/Filler for Polymer; Thermoplastic

Material Notes:
PRE-ELEC ESD 6110 is a static dissipative thermoplastic masterbatch based on PS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 6110 has been developed for injection molding and extrusion of multi-layer sheets for thermoforming. PRE-ELEC ESD 6110 should be used in 40 - 75% ratio with standard HIPS to achieve surface resistance values from 107 to 1010 ohms (EOS/ESD S11.11-1993, IEC 61340-5-1). The products made out of PRE-ELEC ESD 6110 are washable, reusable and recyclable. PRE-ELEC ESD 6110 can also be colored.

Typical applications include injection molded boxes and bins and thermoformed trays and clamshells which give permanent ESD protection for the electronics, medical, pharmaceutical and paper handling industries.

Information provided by Premix Thermoplastics Inc.

Available Properties
  • Density
  • Linear Mold Shrinkage
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Modulus of Elasticity
  • Izod Impact, Unnotched
  • Izod Impact, Notched
  • Surface Resistance
  • Static Decay
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Middle Barrel Temperature
  • Die Temperature
  • Melt Temperature
  • Mold Temperature
  • Roll Temperature
  • Dry Time
  • Moisture Content
  • Injection Pressure
  • Appearance
  • Color
  • Injection Speed
  • Post Pressure, psi
  • Storage Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。