Premix Thermoplastics PREADD AB 171

 

Subcategory: Polyethylene; Additive/Filler for Polymer; Thermoplastic; LDPE

Material Notes:
PREADD AB 171 is an antiblock masterbatch based on synthetic silicate with PE-LD as the carrier polymer. PREADD AB 171 has been developed for applications where an antiblock or matting effect is desired – typically it is being used in the manufacture of polyethylene films.

Due to the good dispersion, purity and fineness of the silicate used, a good antiblocking effect can be achieved already at addition levels of 0.5 %. When using PREADD AB 171 for film matting, an addition of 5-10% is recommended. This addition level does not yet affect negatively on the mechanical properties of the product.

PREADD AB 171 is approved for use in contact with foodstuffs according to FDA and BgVV regulations without limitations.

Information provided by Premix Thermoplastics Inc.

Available Properties
  • Density
  • Additive Loading
  • Maximum Service Temperature, Air
  • Moisture Content
  • Appearance
  • Carrier
  • Color
  • Dosing, %
  • Light Fastness
  • Storage Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。