MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Premix Thermoplastics PREADD PA 143

 

Subcategory: Polyethylene; Additive/Filler for Polymer; Thermoplastic; LLDPE

Material Notes:
PREADD PA 143 is a PE-LLD based processing aid masterbatch for PE-LLD based films. PREADD PA 143 improves processing in conventional PE-LD extruders and specially designed PE-LD extruders when PE-LLD is being run. PREADD PA 143 also improves the extrusion of PE-HD.

The fluoroelastomer additive used in PREADD PA 143 migrates towards metal the surfaces of the extruder enabling the use of narrower die gaps. PREADD PA 143 also reduces wear of the screw and barrel. The pressure in the extruder and the viscosity of the polymer will also be reduced. All this results in increased output as the melt fracture phenomenon appears at higher shear stresses.

PREADD PA 143 is approved for use in contact with foodstuffs according to FDA regulations as long as the dosage of PREADD PA 143 is less than 3 %.

For quick action PREADD PA 143 should be dosed at 30-50 % for the first half an hour (that way the barrel and screw surfaces will be coated quicker with the fluoroelastomer).

Information provided by Premix Thermoplastics Inc.

Available Properties
  • Density
  • Additive Loading
  • Maximum Service Temperature, Air
  • Moisture Content
  • Appearance
  • Carrier
  • Color
  • Dosing, %
  • Storage Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。